PLJ53-60 Chlorinated rubber aluminium paste high-build anti-rust coating

Chlorinated rubber aluminium paste high-build anti-rust coating for marine and underwater steel.

  • For ship bottom, waterline, deck, superstructure.

  • Single-pack; min recoat 12 h at 25°C.

  • Thinner X-15; dilution 3–7%.

PLJ53-60 Chlorinated rubber aluminium paste high-build anti-rust coating Descriotion

Overview
Single-pack chlorinated rubber aluminium paste high-build anti-rust coating with fast drying and thick film build per coat.
Provides anti-rust performance, water resistance, corrosion resistance, and resistance to wet/dry alternation; applicable for low-temperature construction.

Composition
Formulated with chlorinated rubber resin, plasticizer, aluminium paste, anti-rust pigments, solvents, and additives.

Typical uses
For anti-rust protection of ship bottom, waterline, topside, decks, and superstructures.
Also suitable for sluice gates, underwater steel structures, underground pipelines, gas holders, and other steel structures.

Technical data (typical)

  • Appearance: Silver white; aluminium red.

  • Theoretical consumption: 0.22 kg/m² at 60 μm DFT (excluding loss).

  • Density: 1.35 kg/L.

  • Drying time (25°C): Surface dry 1 h; hard dry 12 h.

Application data (25°C)

  • Mixing: Single-pack.

  • Induction time: None.

  • Pot life: Unlimited.

  • Application methods: Airless spray, brush, roller.

  • Thinner: X-15 chlorinated rubber thinner; dilution 3–7%.

  • Recoat interval (25°C): Min 12 h; max unlimited.

  • Recommended coats / DFT: 1 coat 35–50 μm; brush/roller 1 coat 30–40 μm.

Surface preparation
Remove dust, oil, and debris from the previous coat; if beyond maximum recoat interval, consider roughening as needed.
When used as the first coat: blast/shot blast to Sa 2.5 or power-tool cleaning to St 3; surface profile 30–75 μm.

System compatibility / packing / storage

  • Compatibility: Previous coat—epoxy zinc-rich primer; inorganic zinc-rich primer; epoxy intermediate coating; chlorinated rubber primer.

  • Compatibility: Topcoats—chlorinated rubber topcoat; acrylic topcoat.

  • Packing: 20 kg.

  • Storage: Shelf life 12 months; store in a dry, cool place.

Related Products

HUILI anti-rust coatings metal paint pail

CSPE cooling tower damp-proof coating for inner wall anti-corrosion service.

  • For cooling tower inner wall protection.

  • Single-component; min recoat 12 h at 25°C.

  • Resists freeze-thaw, damp heat, and mildew.

HUILI anti-rust coatings metal paint pail

Polyurethane cooling tower damp-proof coating (2K) for waterproof anti-corrosion lining.

  • For cooling towers, sewage tanks, mines, underground buildings.

  • Primer ratio 24:3; topcoat ratio 18:3.

  • Pot life 4 h; min recoat 12 h.

HUILI anti-rust coatings metal paint pail

Premium polyurethane marking coating (2K) for steel structures and concrete chimneys.

  • For chimney marking and protection.

  • Mixing ratio 18:3; pot life 4 h.

  • High gloss; fully hardened 7 d at 25°C.

HUILI anti-rust coatings metal paint pail

Epoxy bitumen cooling tower damp-proof coating (2K) for cooling tower inner wall protection.

  • For cooling towers, sewage tanks, underground mines.

  • Mixing ratio 25:2.5; pot life 4 h.

  • Waterproof, anti-seepage, and mildew resistant.

Contact Us

We would love to speak with you.
Feel free to reach out using the below details.